Creep of Concrete under Variable Stress

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Creep of Concrete under Variable Stress

Author(s): A. D. Ross

Publication: Journal Proceedings

Volume: 54

Issue: 3

Appears on pages(s): 739-758

Keywords: no keywords

DOI: 10.14359/11466

Date: 3/1/1958

Abstract:
Creep has important effects on the st’resses and deflections of reinforced and prestressed structures. Concrete structures in use are subject to variable stress whereas most of the data on creep have been obtained under constant, stress. It is therefore desirable to he able to compute creep under variable stress from the results under constant stress. Three met,hods for doing this are discussed and experimentIs designed to test these methods are described. Each method has a certain advantage in particular circumstances depending on the character of the stress variation, the extent of creep data available, and the accuracy required.