Title: Concrete for Sewage Works

Author(s): E. C. Wenger

Publication: Journal Proceedings

Volume: 54

Issue: 3

Appears on pages(s): 733-738

Keywords: no keywords

DOI: 10.14359/11465

Date: 3/1/1958

Abstract:
Concrete for sewage works and the control of concrete corrosions therein is fully discussed. Characteristics and treatment of sewage are briefly reviewed, along with the conditions of exposure of concrete in such construction. Quality of concrete, construction practices, and other steps necessary to minimize concrete corrosion are presented.