Long-Time Study of Cement Performance in Concrete Chapter 10-Progress Report on Strength and Elastic Properties of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Long-Time Study of Cement Performance in Concrete Chapter 10-Progress Report on Strength and Elastic Properties of Concrete

Author(s): Paul Klieger

Publication: Journal Proceedings

Volume: 54

Issue: 12

Appears on pages(s): 481-504

Keywords: no keywords

DOI: 10.14359/11452

Date: 12/1/1957

Abstract:
This report presents strength data through 3 years for laboratory mortar and concrete specimens made using cements of the Long-Time Study. It also presents information on the elastic properties of the concretes as determined by both static and dynamic means, and pulse velocities as determined by the soniscope.