Proposed Revision of ACI Standard 711-53 Minimum Standard Requirements for Precast Concrete Floor and Roof Units

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed Revision of ACI Standard 711-53 Minimum Standard Requirements for Precast Concrete Floor and Roof Units

Author(s): ACI Committee 711

Publication: Journal Proceedings

Volume: 54

Issue: 12

Appears on pages(s): 441-448

Keywords: no keywords

DOI: 10.14359/11449

Date: 12/1/1957

Abstract:
Minimum standard requirements for single units or multiple element assemblies, to be used in conjunction with ACI 318-56. Covers materials; design principles; manufacture including curing and handling; testing of completed units; installation plans; and special provisions for holes and openings in members. Design chapter treats such problems as dimensions, allowable deflection, structural concrete topping, reinforcement anchorage and location, and use of lightweight concrete.