Title: Temperature Stresses in Continuous Frames

Author(s): Sam Hassid

Publication: Journal Proceedings

Volume: 54

Issue: 11

Appears on pages(s): 415-420

Keywords: no keywords

DOI: 10.14359/11448

Date: 11/1/1957

Abstract:
This paper explains briefly a distribution method useful in analyzing frames subjected to temperature which has been found changes.