Winter Concreting Trends in Europe

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Winter Concreting Trends in Europe

Author(s): E. G. Swenson

Publication: Journal Proceedings

Volume: 54

Issue: 11

Appears on pages(s): 369-384

Keywords: no keywords

DOI: 10.14359/11444

Date: 11/1/1957

Abstract:
Postwar labor and economic problems in Europe have led to governmental encouragement of winter construction. This has resulted in extensive, state-supported research on winter concreting, the progress of which is largely reflected in the papers presented by European authors at the RILEM Symposium on Winter Concreting in Copenhagen, February, 1956. The primary consideration has been the reduction in costs of winter protection of green concrete concurrent with the achievement of better assurance of safety. Research has been directed toward methods of quantitative predic-tion of frost resistance and of minimum protection requirements. Methods of increasing frost resistance of green concrete have received attention. Practical developments involve the refinement of existing methods of safe winter concreting, particularly the choice of building types most suitable for winter construction and the utilization of locally available materials.