Explanatory Notes on Appendix (Ultimate Strength 1 Design) to "Building Code Requirements for Reinforced Concrete (AC I 318156)"*

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Explanatory Notes on Appendix (Ultimate Strength 1 Design) to "Building Code Requirements for Reinforced Concrete (AC I 318156)"*

Author(s): ACI Committee 318

Publication: Journal Proceedings

Volume: 54

Issue: 9

Appears on pages(s): 197-204

Keywords: no keywords

DOI: 10.14359/11437

Date: 9/1/1957

Abstract:
A series of questions and answers on the appendix ("Abstract of Report of ACI-ASCE Joint Committee on Ultimate Strength Design")t to the latest ACI Building Code, AC1 318-56.