Title: Slip-Form Details and Techniques

Author(s): J. F. Camellerie

Publication: Journal Proceedings

Volume: 55

Issue: 4

Appears on pages(s): 1131-1140

Keywords: no keywords

DOI: 10.14359/11410

Date: 4/1/1959

Abstract:
A cursory description of the slip-form construction process - its advantages and limitations. Suggests practical considerations for good results: how to maintain a uniform supply of concrete and a uniform rate of placement; how to keep the construction deck level and walls in vertical alignment; techniques of placing the concrete; and problems of detailing and placing the steel. Surface finishes are also covered, and precautions for winter concreting indicated.




  

Edit Module Settings to define Page Content Reviewer