Continuous Reinforcement In Highway Pavements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Continuous Reinforcement In Highway Pavements

Author(s): ACI Committee 325

Publication: Journal Proceedings

Volume: 55

Issue: 12

Appears on pages(s): 669-678

Keywords: no keywords

DOI: 10.14359/11380

Date: 12/1/1958

Abstract:
A brief description of the continuously reinforced pavements which are now under observation and their performance, a statement of the present status of committee knowledge on the subject of continuous reinforcement, recommendations for future research, and a statement of future plans of the committee.