Proposed ACI Standard Recommended Practice for Hot Weather Concreting*

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed ACI Standard Recommended Practice for Hot Weather Concreting*

Author(s): ACI Committee 605

Publication: Journal Proceedings

Volume: 55

Issue: 10

Appears on pages(s): 525-534

Keywords: no keywords

DOI: 10.14359/11372

Date: 11/1/1958

Abstract:
This recommended practice provides information useful in minimizing detrimental effects of hot weather on concrete. Means are described for reducing concrete temperature by proper attention to ingredients; methods of production and delivery; and care in placement, protection, and curing. Information is given on the use of admixtures to reduce mixing water require-ments and to retard setting. Emphasis is given to the importance of meticulous attention to the use of standard procedures in testing concrete made in hot weather.