Construction for ACI*

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Construction for ACI*

Author(s): John Strang

Publication: Journal Proceedings

Volume: 55

Issue: 10

Appears on pages(s): 431-438

Keywords: no keywords

DOI: 10.14359/11365

Date: 10/1/1958

Abstract:
The general contractor tells of precasting and erection of 46 folded plate sections which comprise the roof of the ACI headquarters building. Concrete mix data are given, and problems of establishing an architecturally satisfactory finish are cited. Cast-in-place fluting of the corridor walls is also discussed.