ACI Standard Minimum Standard Requirements for Precast Concrete Floor and Roof Units (AC1 711-58)*

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ACI Standard Minimum Standard Requirements for Precast Concrete Floor and Roof Units (AC1 711-58)*

Author(s): ACI Committee 711

Publication: Journal Proceedings

Volume: 55

Issue: 7

Appears on pages(s): 83-94

Keywords: no keywords

DOI: 10.14359/11342

Date: 7/1/1958

Abstract:
Minimum standard requirements for single units or multiple element assemblies, to be used in conjunction with AC1 318-56. Covers materials; design principles; manufacture including curing and handling; testing of completed units; installation plans; and special provisions for holes and openings in members. Design chapter treats such problems as dimensions, allowable deflection, structural concrete topping, reinforcement anchorage and location, and use of lightweight concrete.