Proposed Revision of ACI 301-66: Specifications for Structural Concrete for Buildings

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed Revision of ACI 301-66: Specifications for Structural Concrete for Buildings

Author(s): ACI Committee 301

Publication: Journal Proceedings

Volume: 68

Issue: 6

Appears on pages(s): 413-450

Keywords: admixtures: aggregates; air entrainment: architectural concrete buildings: cements; cold weather construction; compressive strength; concrete construction; concrete durability: concrete slabs; concretes; consolidation; conveying.

DOI: 10.14359/11339

Date: 6/1/1971

Abstract:
These specifications are a reference standard which the engineer or architect may make applicable to any building project by citing them in the project specifications. He supplements them as needed by designating or specifying individual project requirements. The document covers materials and proportioninq of concrete reinforcing and Prestressing steels: production, placing, and curing of concrete and formwork design and construction. Methods of treatment of ioints and embedded items air of surface defects, and finishing of formed surfaces are specified. Separate chapters are devoted to slab construction and finishing, architectural concrete massive concrete, and materials and methods for constructing post-tensioned concrete. Provisions governing testing, evaluation, and acceptance of concrete as well as for acceptance of the structure are included.