Comparative Study of Prestressed Concrete Beams, With and Without Bond

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Comparative Study of Prestressed Concrete Beams, With and Without Bond

Author(s): Alan H. Mattock, Jun Yamazaki, and Basil T. Kattula

Publication: Journal Proceedings

Volume: 68

Issue: 2

Appears on pages(s): 116-125

Keywords: beams (supports);bond (concrete to reinforcement);continious beams;crack width and spacing;deflection;moments;post-tensioning;prestressed concrete;reinforced concrete;research;serviceablity;strength;T-beams; unbonded prestressing.

DOI: 10.14359/11298

Date: 2/1/1971

Abstract:
Tests were made of seven simple span beams of 28-ft span, and of three beams continious over two spans of 28 ft each. The primary variables were, the presence or absence of bond; the amount of bonded unprestresses reinforcement; and the use of seven wire strand as unbonded prestressed reinforcement. The unbonded post-tensioned beams with minimum reccomended unprestressed bonded reinforcement had serviceablity chasrateristics, strength, and ductility equal to, or better than, those of compareable bonded post-tensioned beams. An expression is proposed for the ultimate stress in unbonded tedons. Seven wire strand can be used effectively as unprestressed bonded reinforcement.