Microcracking Effect on Flexural Strength of Concrete After Repeated Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Microcracking Effect on Flexural Strength of Concrete After Repeated Loading

Author(s): Akira Yoshimotot, Shoji Ogino, and Masashi Kawakami

Publication: Journal Proceedings

Volume: 69

Issue: 4

Appears on pages(s): 233-240

Keywords: bond (paste to aggregate);cement pastes;concretes;crack propagation;cyclic loads;fatigue (materials);flexural strength;fracture mechanics;Griffith crack; microcracking;microscopy;microstructure;research.

DOI: 10.14359/11268

Date: 4/1/1972

Abstract:
The purpose of this investigation was to study the flexural strength of concrete beam specimens after repeated loading. The test results showed that some specimens produced an increase in flexural strength after repeated loading. An attempt is made to explain this strength increase. It appears likely that microcracking propagation is responsible for this increase in flexural strength.