Prediction of Concrete Creep Effects Using Age-Adjusted Effective Modulus Method

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Prediction of Concrete Creep Effects Using Age-Adjusted Effective Modulus Method

Author(s): Zdenek P. Bazant

Publication: Journal Proceedings

Volume: 69

Issue: 4

Appears on pages(s): 212-219

Keywords: age;concretes;creep properties;deflection;modulus of elasticity;prestress loss; relaxation (mechanics);shirnkage;stresses;structural analysis.

DOI: 10.14359/11265

Date: 4/1/1972

Abstract:
A recently proposed refinement of the effective modulus method, accounting for concrete agins, is formulated in a rigorus form and is extended to allow for the variation of an elastic modulus and an unbounded final value of creep. A numerical example is included to show the application of the proposed method in predicting creep effects.