Bleeding in Concrete- A Microscopic Study

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Bleeding in Concrete- A Microscopic Study

Author(s): John E. Ash

Publication: Journal Proceedings

Volume: 69

Issue: 4

Appears on pages(s): 209-211

Keywords: anisotropy;bleeding (concrete);concretes;deformation;durablity; microcracking; microscopy;microstructure;research;tensile strength;tension tests.

DOI: 10.14359/11264

Date: 4/1/1972

Abstract:
Bleeding can have far-reaching effects on the preparation of concrete and it’s a phenomenon which has too often been ignored. This paper briefly discusses some of its important consequences with particular emphasis on tensile strength and deformational behavior, and suggests a method by which effects of bleeding on the internal structure of concrete may be studied.