Title: New Developments in the Use of Concrete Conveyors

Author(s): James L. Cope

Publication: Journal Proceedings

Volume: 69

Issue: 4

Appears on pages(s): 201-208

Keywords: concrete construction;concretes;construction equipment;conveying;materials handling;placing.

DOI: 10.14359/11263

Date: 4/1/1972

Abstract:
Reviews the development of conveyor systems for effective plaing of ready-mixed concrete. The techniques for using belt conveyors in this manner over the last 15 years, special conveyors developed, are discussed. Three types of conveyors are described: portable units for short lift and short reach applications, feeder units for spreading applications, and side discharge units for spreading applications.