Heat Resistant Portland Cement Concrete to Withstand Combined High Temperatures and Structural Loads

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Heat Resistant Portland Cement Concrete to Withstand Combined High Temperatures and Structural Loads

Author(s): Joesph N. David

Publication: Journal Proceedings

Volume: 69

Issue: 2

Appears on pages(s): 118-124

Keywords: bricks;clays;corse aggregates;compressive strength;concrtes;density (mass/ volume);dynamic modulus of elasticity;expanded shale aggregate;fireclays;high temperature;lightweight aggregate concretes;pre-placed aggregate concrete; research;tensile strength.

DOI: 10.14359/11257

Date: 2/1/1972

Abstract:
Observations from tests show that reductions in strength, and changes in physical properties, that occur in portland cement concrete as a result of cyclic heat to 600 F (316 C), can be accurately evaluated and accomodated into a fesible design for a concrete structure. The preliminary test results, developed for the concrete used in the support for a reactor vessel, show the significance in the cement factor for achieving the least amount of deterioration due to high temperature cycling, with special reference to heat resistant corse aggregate mixes.