Grouting Program for Pile Repairs - Portuaria Automata, Acajutia, El Salvador

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Grouting Program for Pile Repairs - Portuaria Automata, Acajutia, El Salvador

Author(s): S. R. Annet

Publication: Journal Proceedings

Volume: 69

Issue: 1

Appears on pages(s): 55-60

Keywords: caissons; concrete construction; concrete piles; concretes; demolition; foun-dations;grouting: harbor structures; piers; repairs.

DOI: 10.14359/11249

Date: 1/1/1972

Abstract:
From 1967 to 1970 an automated pier was built for the Comision Ejecutiva Portuaria Automata, at Acajutla, El Salvador. The pier was founded on piles sunk into volcanic tuff which is the rock native to the area. The final load testing program resulted in unacceptable settlement of certain piles, in excess of 0.4 in. (9 mm) and up to 2.1 in. (54 mm). A drilling and coring program revealed the following defects: 1. Segregation of coarse aggregate, sand, and cement in the concrete in the pile, or 2. Unstable ground at the base of the pile, or 3. Some combination of Defects I and 2. Water pressure testing following the drilling and coring program indicated that some grout collars between the piles and the volcanic tuff had been broken by the settlement.