Construction Considerations for Serviceable Concrete Floors

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Construction Considerations for Serviceable Concrete Floors

Author(s): George Frey

Publication: Journal Proceedings

Volume: 70

Issue: 6

Appears on pages(s): 416-419

Keywords: carbonation: cold weather construction: concrete construction;concrete slabs: concretes:concrete finishing (fresh concrete] :finishes; floors; hot weather construction;placing: quality control: repairs: salamanders.

DOI: 10.14359/11220

Date: 6/1/1973

Abstract:
Construction considerations for concrete floors are innumerable. A contractor looks at all the factors, ranging from the selection of ready-mixed concrete suppliers to remedial work of damaged floor slabs. Discussion is devoted to materials, placing and finishing techniques, job planning, tolerances, cold weather concreting, hot weather concreting, and repair.