Preliminary Design and Proportioning of Relnforced Concrete Bridge Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Preliminary Design and Proportioning of Relnforced Concrete Bridge Structures

Author(s): ACI Committee 443

Publication: Journal Proceedings

Volume: 70

Issue: 5

Appears on pages(s): 328-336

Keywords: arch bridges; beams (supports); box beams; bridge abutments; bridge decks; bridge foundations: bridge piers; bridges (structures) ; girders; precast concrete; prestressed concrete:reinforced concrete; structural design;suspension bridges; T-beams.

DOI: 10.14359/11214

Date: 5/1/1973

Abstract:
To fulfill a portion of its stated mission to "develop recommended practices for structural design of concrete bridges on the basis of the most up-to-date information," ACI Committee 443, Concrete Bridge Design, is publishing for discussion chapters of what will eventually be a complete recommended practice. At this time, the information is only being considered for adoption by the committee. Therefore, it is still subject to revision.