Design Aids for the Direct Design Method of Flat Slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design Aids for the Direct Design Method of Flat Slabs

Author(s): Alfred Zweig

Publication: Journal Proceedings

Volume: 70

Issue: 4

Appears on pages(s): 285-299

Keywords: bays (structural bending units) ; beams (supports); bending moments; caps (supports) ; columns (supports);concrete slabs; flat concrete plates: multistory buildings;reinforced concrete; structural analysis: structural design.

DOI: 10.14359/11209

Date: 4/1/1973

Abstract:
The purpose of this paper is to present aids for the design of flat slabs and flat plates by the Direct Design Method, as outlined in Chapter 13 of ACI 318-71. The use of the aids is demonstrated by two practical examples.