Michigan’s Experience with Neoprene Compression Seals

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Michigan’s Experience with Neoprene Compression Seals

Author(s): Leroy T. Oehler and Francis J. Bashore

Publication: Journal Proceedings

Volume: 70

Issue: 3

Appears on pages(s): 214-220

Keywords: bridge decks; concrete construction; concrete pavements; contraction; control joints; deterioration; expansion: fatigue (materials); joint fillers; joint sealers; joints (junctions) ; specifications.

DOI: 10.14359/11200

Date: 3/1/1973

Abstract:
Reviews the experience of the Michigan Department of State Highways with the use of neoprene compression seals. Field experience and research that led to the development of specifications for their use are described. The specifications are discussed and a summary of regu ar condition sur-veys on sealed joints is presented.