Behavior of Reinforced Columns Subjected to Fatigue Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Reinforced Columns Subjected to Fatigue Loading

Author(s): Knut Aas-Jakobsen and Rolf Lenschow

Publication: Journal Proceedings

Volume: 70

Issue: 3

Appears on pages(s): 199-206

Keywords: axial loads; columns (supports) ;cyclic loads; deformation; fatigue (materials); flexural strength; loads (forces);strains.

DOI: 10.14359/11198

Date: 3/1/1973

Abstract:
The behavior of I I columns has been studied experimentally and analytically. A numerical method computing deformation of columns under fatigue loading is proposed.