Commentary on Recommended Practice for Design and Construction of Concrete Bins, Silos, and Bunkers for Storing Granular Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Commentary on Recommended Practice for Design and Construction of Concrete Bins, Silos, and Bunkers for Storing Granular Materials

Author(s): ACI Committee 313

Publication: Journal Proceedings

Volume: 72

Issue: 10

Appears on pages(s): 549-565

Keywords: bins;concrete;concrete construction;dead loads;dynamic loads;earthquake resistant structures;formwork (construction);granular materials;lateral loads; loads(forces);overpressure;quality control;reinforced concrete;reinforcing steels;silos.

DOI: 10.14359/11156

Date: 10/1/1975

Abstract:
Presents some of the considerations and assumptions of ACI Committee 313 in developing the provisions of the "Recommended Practice for the Design and Construction of Concrete Bins, Silos, and Bunkers for Storing Granular Materials." It also provides suggested methods for calculating crack width, through-the-wall temperture gradient due to hot stored materials and the effect of eccentric discharge. Comments on specific provisions of the recommended practice are made using the corresponding chapter and section numbrs of the recommended practice. A list of selected references is given at the end of the commentary.