Torsional Strength of Longitudinally Reinforced Beams Containing an Opening

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Torsional Strength of Longitudinally Reinforced Beams Containing an Opening

Author(s): A. E. McMullen and H. R. Daniel

Publication: Journal Proceedings

Volume: 72

Issue: 8

Appears on pages(s): 415-420

Keywords: angle of twist;beams (supports);bending moments;cracking (fracturing); deflection; deformation; loads (forces);openings;reinforced concrete; shear properties;strains;structural design;torsion;torsion tests.

DOI: 10.14359/11144

Date: 8/1/1975

Abstract:
Equations for predicting the torsional strength of longitudinally reinforced concrete beams that contain an opening to accommodate service ducts are presented and the results are compared with the test results of 29 beams. The strength of beams containing a short opening can be significantly larger than the strength predicted by the theory because the spiral crack extends into the solid portion of the beam. However, the eqautions can be modified emprically so that they satisfactorily predict the torsional strength. Although all the beams tested were subjected to pure torsion, the analysis includes the shear and moment due to self weight of the beam and can thus easily be extended to include members supporting external loads that cause shear and bending.