Concrete Formwork Failures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Formwork Failures

Author(s): Jacob Field

Publication: Journal Proceedings

Volume: 72

Issue: 7

Appears on pages(s): 351-355

Keywords: concretes;failure;finishes; formwork (construction);foundations;lateral pressure; loads (forces);parting agents;pressure;settlement (structural);shoring; wind pressure.

DOI: 10.14359/11141

Date: 7/1/1975

Abstract:
The cause of most formwork failures is not discovered because the rubble covers the strategic information and seldom is the exposure made carefully enough to permit proper obsevation and measurement. Repetitive failure patterns and careful collection of information in several incidents hows a similarity of cause. The avoidance of such detail can reduce the number of future failures. Investigation of reported formwork failures often proves that the proximate cause was not in the formwork but in the structure or foundation supporting the formwork. The forms collapsed even though structurally sufficient. They collapsed because the supporting structure failed or settled differentially.