Title: Cathodic Protection: 12 Years Later and Counting

Author(s): Kermit D. Bright

Publication: Concrete International

Volume: 23

Issue: 12

Appears on pages(s): 73-75

Keywords:

DOI:

Date: 12/1/2001

Abstract:
Concrete parking structures are often plagued by reinforcement corrosion that leads to expensive repairs. One option promoted to solve this problem is cathodic protection (CP). But how well does it work?