Thermal Relaxation in Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Thermal Relaxation in Concrete Structures

Author(s): Jim Pajuhesh

Publication: Journal Proceedings

Volume: 73

Issue: 9

Appears on pages(s): 522-525

Keywords: cracking (fracturing): deformation; loads (forces) : modlus of elasticity: nuclear reactor containment:reinforced concrete: reinforcinq steels: relaxation (mechan-ics);strains: stress-strain relationships: stresses: ;structural analysis; tensile stresses.

DOI: 10.14359/11094

Date: 9/1/1976

Abstract:
A solution is developed to investigate the cracking, thermal relaxation, and resulting strains and stresses in a given reinforced concrete section under any specified temperature distribution and any combination of force and moment, The thermal relaxation is based on the choice of various porsibilities for structural behavior under thermal loading. The options considered include the condition of free expansion or rotation, complete restraint against either or both, as well as the general case of a given combination of two types of effects: a set of force and moment to be sustained and unaffected by cracking, and a specified set of middle surface strain and curvature with the corresponding force and moment relaxed through concrete cracking and plasticity. The criteria and equations for review of the section and evaluation of thermal relaxation are presented for parabolic concrete stress-strain relation. Other possibilities can be treated in a similar fashion.