Detailing for Torsion

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Detailing for Torsion

Author(s): Denis Mitchell and Michael P. Collins

Publication: Journal Proceedings

Volume: 73

Issue: 9

Appears on pages(s): 506-511

Keywords: anchorage (structural); beams (supports) ;cover; cracking (fracturing): crack width and spacing: detailing;reinforced concrete: reinforcing steels; spalling; stirrups: structural design; torsion.

DOI: 10.14359/11091

Date: 9/1/1976

Abstract:
This paper discusses the detailing af torsional reinforcement. First, the functions of the longitudinal and transverse torsional steel are explained in terms of a simple, easy to visualize model. After introducing the concept of spalling of the concrete cover, the detailing requirements which are necessary if the reinforcement is to fulfill its functions are presented. The consequences of incorrect detailing are discussed.