Proposed Revision of ACI 214-65: Recommended Practice for Evaluation of Strength Test Results of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed Revision of ACI 214-65: Recommended Practice for Evaluation of Strength Test Results of Concrete

Author(s): ACI Committee 214

Publication: Journal Proceedings

Volume: 73

Issue: 5

Appears on pages(s): 265-278

Keywords: coefficient of variation;compressive strength;concrete construction; cylinders;quality control;sampling;standard deviation;statistical analysis; variations.

DOI: 10.14359/11072

Date: 5/1/1976

Abstract:
Statistical procedures provide valuable took for assessing results of strength tests, and such an approach is also of value in refining design criteria and specifications. The report discusses briefly the numerous variations that occur in the strength of concrete and presents statistical procedures which are useful in interpreting these variations.