Epoxy Adhesives in Prestressed and Precast Concrete Bridge Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Epoxy Adhesives in Prestressed and Precast Concrete Bridge Construction

Author(s): Raymond J. Schutz

Publication: Journal Proceedings

Volume: 73

Issue: 3

Appears on pages(s): 155-159

Keywords: adhesives; bridge decks; bridges (structures);compressive strength;concrete construction; creep properties;epoxy resins; precast concrete;prestressed concrete;modulus of elasticity; shear connectors;shear properties;shear strength; tensile strength.

DOI: 10.14359/11064

Date: 3/1/1976

Abstract:
The use of epoxy resin based adhesives in two different types of precast concrete bridge construction are described. The bridges covered are the conventional segmental bridges and a new system of precast concrete bridge deck construction. Construction procedures are described, and the physical properties of the different types of adhesives required are reviewed.