Stressed State Analysis of Concrete Walls

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Stressed State Analysis of Concrete Walls

Author(s): F. Bljuger

Publication: Journal Proceedings

Volume: 74

Issue: 7

Appears on pages(s): 288-293

Keywords: bearing capacity; bearing walls; bending moments;deformation; modulus of elasticity; precast concrete;strains: stress analysis; stress-strain relationships; stresses;structural analysis; walls.

DOI: 10.14359/11013

Date: 7/1/1977

Abstract:
The influence of the real stress-strain diagram of concrete wall structures on stress distributions and ultimate moments is considered. The stress-strain diagrams taken for the analysis are based on special experimental data. Consideration of the real diagrams permits an increase of the wall bearing capacity under horizontal loading by IO to 25 percent.