Title: Revisions to Guide to Joint Sealants for Concrete Structures

Author(s): ACI Committee 504

Publication: Journal Proceedings

Volume: 74

Issue: 6

Appears on pages(s): 238-255

Keywords: bridge decks;concrete construction;concrete panels;concrete pavements; construction joints;control joints;isolation joints;joint fillers;joint sealers; joints (junctions);precast concrete; sealers; specifications.

DOI: 10.14359/11009

Date: 6/1/1977

Abstract:
Updates the I970 report "Guide to Joint Sealants for Concrete Structures". Corrections and changes to that report are listed and new developments in field-molded and preformed sealants and their use are described. A new Appendix C provides a list of specifications.