Tests to Establish Concrete Pumpability

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tests to Establish Concrete Pumpability

Author(s): Roger D. Browne and Phillip B. Bamforth

Publication: Journal Proceedings

Volume: 74

Issue: 5

Appears on pages(s): 193-203

Keywords: concretes;field tests; fresh concretes; mix proportioning;permeability;pumped concrete; pumping; pumps;test equipment; tests; voids; water;water-cement ratio;workability.

DOI: 10.14359/11001

Date: 5/1/1977

Abstract:
This paper describes test methods developed for examining the pumping characteristics of concrete which have aided the range of studies undertaken on pumped concrete over the last 8 years. Details are given of the basic state of the concrete in the pipeline, from which is established the importance of impermeability of the material in minimizing pipe blockage. A practical test method for this property, simulating the pressurized state of concrete in a pipeline, is described, together with test results from pumping trials on a number of concrete mixes. Viscometric methods are also briefly mentioned in relation to the laboratory measurement of flow resistance. The void meter test is described and its value as a mix proportioning tool is considered in relation to the optimization of cement contents. Finally, the details and results from instrumen-ation of pipelines to observe pumping pressure variations are presented and conclusions are given related to pump performance and concrete characteristics.