Prediction of the Thermal Coefficient of Expansion of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Prediction of the Thermal Coefficient of Expansion of Concrete

Author(s): Jack H. Emanuel and J. Leroy Hulsey

Publication: Journal Proceedings

Volume: 74

Issue: 4

Appears on pages(s): 149-155

Keywords: age;aggregates; bridges (structures);cement pastes: concretes; expansion; fineness; limestone; mix proportioning; moisture content; portland cements; temperature;thermal expansion: thermal properties; thermal stresses;volume change.

DOI: 10.14359/10996

Date: 4/1/1977

Abstract:
A review of the literature identifies age, moisture content, and proportion of the mix as the principal factors affecting the thermal coefficient of expansion of concrete. From the discussion, correction factors and an empirical equation are developed which take into account these factors. Coefficients are calculated for twelve sets of reported data and compare favorably with the reported values. Although the resultant values would be subject to fluctuation resulting from environmental effects, the equation provides a realistic value for design consideration of thermal movements and resultant stresses.




  