Durability of Palm-Tree Frond Fiber Reinforcement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Durability of Palm-Tree Frond Fiber Reinforcement

Author(s): M. Samir Abdel-Azim

Publication: Concrete International

Volume: 17

Issue: 6

Appears on pages(s): 27-31

Keywords: construction materials; composite materials; cracking; durability; fiber reinforced concretes; Materials Research

DOI:

Date: 6/1/1995

Abstract:
Palm tree fronds (PTF), as natural fibers have many good characteristics that make it suitable for the enhancement of the characteristics of cement-based composites to be used economically in the construction of houses. In the present work, physical, mechanical and chemical tests were carried out to examine the durability of PTF. Also the effect of adding PTF leaf fibers to concrete was studied and was found to be suitable to improve the tensile strength and workability of concrete.