Title: Proposed ACI Standard 503.4: Standard Specification for Repairing Concrete with Epoxy Mortars

Author(s): ACI Committee 503

Publication: Journal Proceedings

Volume: 75

Issue: 9

Appears on pages(s): 454-459

Keywords: bond (concrete to concrete);concrete construction;epoxy resins; hardened concrete;mortars (material);quality control;repairs;resurfacing;specifications; standards.

DOI: 10.14359/10960

Date: 9/1/1978

Abstract:
this specification describes the work of repairing defects in hardened portland cement concrete with a sand-filled morar using an adhesive binder such as defined in ASTM C881. It includes controls for adhesive labeling,storage, handeling, mixing and applcation, surface evaluation and preparation, as well as inspection and quality control.