How Good is Good Enough-A Dilemma in Acceptance Testing of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: How Good is Good Enough-A Dilemma in Acceptance Testing of Concrete

Author(s): H. W. Chung

Publication: Journal Proceedings

Volume: 75

Issue: 8

Appears on pages(s): 374-380

Keywords: acceptability; building codes; compressive strength: concretes; mix proportioning; quality control.

DOI: 10.14359/10951

Date: 8/1/1978

Abstract:
Compliance with concrete strength level requirements is usually judged by an acceptance test. The criteria of acceptance stipulated in ACI 3 18- 71, as well as the British and Australian codes, are reviewed and their efficiencies are compared by means of the operating characteristic curves. It is shown that the ACI 3 18-71 criteria involve a low producer’s risk but a very high consumer’s risk, with the effect that "good" concrete is always accepted but "poor" concrete may not be detected. A revision of the criteria is proposed whereby the risk is distributed more evenly between the two parties.