Properties of Fiber Reinforced Shrinkage-Compensating Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Properties of Fiber Reinforced Shrinkage-Compensating Concrete

Author(s): B. K. Paul, M. Polivka, and P. K. Mehta

Publication: Journal Proceedings

Volume: 78

Issue: 6

Appears on pages(s): 488-492

Keywords: compressive strength; expansive cement concretes: fiber reinforced concretes; flexural strength; metal fibers; modulus of elasticity; portland ce-ments;shrinkage-compensating concretes; strength.

DOI: 10.14359/10927

Date: 11/1/1981

Abstract:
Tests were carried out with two types of steel fibers to evaluate their restraining capability in shrinkage-compensating concrete. The effect of the fiber reinforcement on compressive flexural strength and modulus of elasticity was investigated. The results indicate that steel fibers can be successfully used for restraining shrinkage-compensating cement. Inclusion of fibers in concrete improved the compressive and flexural strength of both plain and conventionally reinforced shrinkage-compensating concretes. The differences in the moduh were insignificant for practical purposes. Concrete containing bent fibers showed less restrained expansion and higher flexural strength when compared to concrete with straight fibers.




  