Re-examination of the Relation Between Splitting Tensile and Compressive Strength of Normal Weight Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Re-examination of the Relation Between Splitting Tensile and Compressive Strength of Normal Weight Concrete

Author(s): Nicholas J. Carino and H. S. Lew

Publication: Journal Proceedings

Volume: 79

Issue: 3

Appears on pages(s): 214-219

Keywords: age-strength relation; building codes; compressive strength; concretes;regression analysis; safety; shear properties; splitting tensile strength;statistical analysis.

DOI: 10.14359/10900

Date: 5/1/1982

Abstract:
Based on statistical analyses of selected data, which included concretes with compressive strengths from 980 psi (6.9 MPa) to 5750 psi (39.7 MPa), it is shown that the commonly assumed square root of compressive strength function is not the most appropriate relation for selected data or data with a similar precision and the same range; rather, a simple power function is more applicable over a wide range of concrete strengths.