Serviceablity Behavior and Failure Mechanisms of Concrete Inverted T-Beam Bridge Bentcaps

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Serviceablity Behavior and Failure Mechanisms of Concrete Inverted T-Beam Bridge Bentcaps

Author(s): Sher Ali Mirza and Richard W. Furlong

Publication: Journal Proceedings

Volume: 80

Issue: 4

Appears on pages(s): 294-304

Keywords: bents; bridges (structures); caps (supports); failure mechanisms; flanges; prestressed concrete; reinforced concrete; serviceablity; stirrups; T-beams.

DOI: 10.14359/10850

Date: 7/1/1983

Abstract:
Structural behavior of inverted T-beams diffem from thaf of the more conventional top-loaded standard T-section. The response of prestressed members may be significantly different from that of reinforced members. Due to the iack of recommendation available for the design of beams to resist torsion, this study was conducted to provide data for designing both conventional and prestressed concrete inverted T-beam bentcaps with special attention to web reinforcement, both the amount and location of stirrups; service load cracking in response to equal and opposite torsions due to traffic toads; strength and stiffness of web and flange as the amount of combined texure, shear, and torsion increases to the maximum capacity. Strength and serviceability behavior of inverted T-beams bentcaps is also examined with emphasis on experimental study.