Serviceability Provisions in the New Eurocode for the Design of Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Serviceability Provisions in the New Eurocode for the Design of Concrete Structures

Author(s): A. W. Beeby

Publication: Symposium Paper

Volume: 203

Issue:

Appears on pages(s): 15-32

Keywords: beams; code provisions; deflection control; Eurocode; serviceability; stress checks

DOI: 10.14359/10802

Date: 8/1/2001

Abstract:
This paper provides an outline of the provisions for design for serviceability given in the current version of Eurocode 2; the Eurocode for the design of concrete structures. The provisions for stress limitation and crack control are outlined briefly together with some of the reasoning behind them. A more detailed description of the background and content of the clauses dealing with the control of deflection are given.