Influence of Synthesis Temperature on the Hydration of New Cements from Fly Ash of Municipal Solid Waste Incineration

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Synthesis Temperature on the Hydration of New Cements from Fly Ash of Municipal Solid Waste Incineration

Author(s): A. Guerrero, S. Goi, A. Macias, E. Fernhdez, and M. P. Lorenzo

Publication: Symposium Paper

Volume: 202

Issue:

Appears on pages(s): 267-284

Keywords: cement; fly ash; hydration; incineration; municipal solid-waste

DOI: 10.14359/10788

Date: 8/1/2001

Abstract:
The influence of the synthesis temperature on the hydration reaction of new cements obtained from municipal solid waste incineration fly ash (MSWIFA), as a secondary raw material, is discussed in this work. Cements were synthesized in a range of temperature between 700°C and 1400°C from MSWIFA, which was previously activated by hydrothermal treatment at 200°C and 1.24 MPa. The evolution of cemented phases with the heating temperature was followed by X-ray difiaction (XRD) and infrared spectrometry (IR). The results were compared with those obtained by heating the starting fly ash without hydrothermal treatment. The degree of hydration was semi-quantitatively evaluated by XRD, during a period of 28 days, in cements obtained at low temperatures (7OOC, SOO’C, 9OOC, 1000°C and 11 OO°C).