Use of Recycled Concrete as Aggregates for the Construction of Fish Reefs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Use of Recycled Concrete as Aggregates for the Construction of Fish Reefs

Author(s): T. Yen, K. H. Chen, and Y. W. Liu

Publication: Symposium Paper

Volume: 202

Issue:

Appears on pages(s): 197-206

Keywords: earthquake; fish reef; recycled aggregate; recycled concrete

DOI: 10.14359/10782

Date: 8/1/2001

Abstract:
As a result of the Chi-Chi earthquake, which occurred in middle Taiwan on September 2 1, 1999, numerous buildings and bridges were seriously damaged. How to reuse a huge amount of building debris collected from the damaged structures became an important issue. After being crushed and screened, this debris could be served as recycled aggregate in concrete. Such recycled concrete is recommended to be used for sub-structures or other applications. Therefore, the production of fish reefs became one of the possibilities. In the study, treatment and measurement of the basic properties of the recycled aggregates were firstly studied. Then manufacture fish reef with the recycled concrete were undertaken. Test results show that the properties of recycled aggregate can meet the requirements of natural aggregate. The fish reefs produced by using the recycled concrete were satisfactory and conformed to the demands of the Fisheries Administration in Taiwan.