The Fracture Surface Roughness of Concrete with Different Aggregate Sizes and loading Rates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Fracture Surface Roughness of Concrete with Different Aggregate Sizes and loading Rates

Author(s): Y.-S. Roh and Y. Xi

Publication: Symposium Paper

Volume: 201

Issue:

Appears on pages(s): 35-54

Keywords: aggregate size; fractal; fracture; loading rate; mug hness

DOI: 10.14359/10757

Date: 7/1/2001

Abstract:
Fracture surface provides valuable information on internal structure and mechanical behavior of composite materials. Loading rate affects the roughness of the fracture surface of composites. A higher loading rate, in general, results in a smoother fracture surface. Similarly, aggregate size influences the roughness of the fracture surface. Larger aggregates cause a rougher fracture surface under the same loading rate. The roughness of the fracture surface of concrete is experimentally studied using concrete specimens made of the different aggregate sizes under different loading rates. Fractal dimension is used to evaluate the surface roughness of concrete specimens. A new fractal fracture model is developed which correlates the fractal dimension with concrete mix design parameters, such as volume fraction and size of aggregate, as well as loading rate. The model prediction agrees with test data very well.