Who Really Cares About Building Codes?

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Who Really Cares About Building Codes?

Author(s): John V. Loscheider

Publication: Concrete International

Volume: 23

Issue: 9

Appears on pages(s): 62-65

Keywords:

DOI:

Date: 9/1/2001

Abstract:
To maintain appropriate influence over our building codes, we must recognize that there are others besides structural engineers who care about the structural provisions.