Concrete Frame Corners

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Frame Corners

Author(s): Erik Skettrup, Jorgen Strabo, Niels Houmark Andersen, and Troels Brondum-Nielsen

Publication: Journal Proceedings

Volume: 81

Issue: 6

Appears on pages(s): 587-593

Keywords: bending moments; corner joints; frames; loads (forces); reinforced concrete;reinforcing steels; tests.

DOI: 10.14359/10704

Date: 11/1/1984

Abstract:
Tests on reinforced concrete frame corners subjected to an opening bending moment (corresponding to tensile stresses in the reentrant corner) are described. Three fundamentally different reinforcement arrangements were tested. For high percentages of reinforcement, the load-carrying capacity of a common reinforcement arrangement proved to be low. Modified reinforcement arrangements resulted in corners that could transfer the same bending moments as the adjacent beams, even with balanced reinforcement.