Evaporation of Water from Fresh Mortar and Concrete at Different Environmental Conditions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaporation of Water from Fresh Mortar and Concrete at Different Environmental Conditions

Author(s): Zawde Berhane

Publication: Journal Proceedings

Volume: 81

Issue: 6

Appears on pages(s): 560-565

Keywords: age; environments; evaporation; fresh concretes; hot weather construction; humidity; mortars (material); temperature; water-cement ratio; water content.

DOI: 10.14359/10700

Date: 11/1/1984

Abstract:
The effect of different environmental conditions on the rate and amount of water evaporation from fresh mortar and concrete surfaces was investigated. The variables studied were air temperature, initial mortar and concrete temperature, wind speed, relative humidity, type of cement, and water content (water-cement ratio). The results show that in hot, humid climate evaporation is 3 1/2 times lower than in a hot, moderate climate and 7% times lower than in a hot, dry climate. There is an indication that Menzel’s formula may not be applicable for estimating evaporation rate at any stage of fresh mortar or concrete in any climatic conditions.